  • Quais são as medidas anti-alojamento comuns para os parafusos e suas características?

Spring washer anti-loosening is simple and easy to implement. It generates pre-tightening force through the elastic deformation of the washer, with low cost but general anti-loosening effect, suitable for parts with small vibration. Double nut anti-loosening produces friction through the mutual extrusion of two nuts, with reliable anti-loosening effect but increased weight and cost, often used in important connection parts such as turnouts. Spiralock thread anti-loosening increases friction by using a special tooth profile, without additional parts, with long-lasting anti-loosening effect, suitable for high-speed and heavy-haul railway bolts. Spot welding anti-loosening fixes the nut and bolt by welding, with thorough anti-loosening effect but difficult disassembly, only used in parts that are not frequently Desmontado . Anti-alojamento adesivo Aplica adesivo anaeróbico no fio, que forma um filme de cola após a cura para evitar afrouxamento, destacável e com bom efeito anti-alojamento, amplamente utilizado em parafusos de pista .}}}}}}

 

rail bolt in railway

 

  • Quais são as formas comuns de falha do parafuso e como identificá -las?

Fatigue fracture is the most common form, with obvious fatigue lines and instantaneous fracture areas on the fracture surface, mostly occurring at the transition between the bolt head and the shank, which can be detected by flaw detection. Tensile fracture is characterized by a flat fracture surface without fatigue lines, often caused by excessive pre-tightening force or insufficient material strength, which can be identified by measuring the fracture diameter. Thread slippage is manifested as wear or deformation of the thread profile, unable to be tightened, which can be judged by a thread gauge when the profile deviation exceeds 0.2mm. Corrosion failure is shown as rust on the bolt surface, and in severe cases, rust pits and reduced cross-section, which can be identified by visual inspection and A medição da espessura e os parafusos precisam ser substituídos quando a profundidade da ferrugem exceder 5% do diâmetro original.

 

spike in stock

 

  • Quais são as principais causas da falha do parafuso?

O controle de força de pré-aperto inadequado é uma razão importante . força de pré-aperto excessiva excedendo a força de escoamento do parafuso, levará à fratura por tração de parafuso; A força de pré-aperto insuficiente não pode impedir efetivamente o afrouxamento, e o parafuso é fácil de soltar sob vibração, levando à falha . materiais não qualificados fará com que o desempenho do raio, como a resistência, como a requisito de projeto, como a necessidade de que a inspeção de gravação e outros defeitos, que são fáceis de quebrar, a inspeção de material é necessária {5 {5 de defesa, a inspeção de tais, 5, a inspeção de gravação e outros defeitos, que é fácil, a inspeção do material, que a inspeção do material é necessária, e a inspeção do material é necessária, e a inspeção de gravação, que é necessária, a inspeção de gravação e outros defeitos, que é fácil, a inspeção de gravação, a inspeção de material, e a inspeção do material, a inspeção do material, e a inspeção do material e a inspeção do material. and cracks are easy to generate at the damaged part under alternating load, eventually leading to failure. Environmental corrosion will damage the bolt surface, especially in humid and salt-fog environments. Rust will weaken the bolt cross-section and reduce the bearing capacity, and long-term corrosion will lead to bolt failure. Fatigue load is a long-term factor. The A carga alternada gerada por operação do trem faz com que a tensão do parafuso e a força de cisalhamento repetidamente . quando exceder o limite de fadiga, as rachaduras de fadiga serão geradas e se expandem gradualmente para fraturas .

 

spike in railway

 

  • Como melhorar o projeto do parafusos e o uso por meio da análise de falhas?

Analyze the fracture surface of the failed bolt to determine the fracture type (fatigue, overload, etc.). If it is fatigue fracture, the bolt diameter can be increased or high-strength materials can be used to improve its fatigue strength. Adjust the pre-tightening force standard according to the failure cause. If the fracture is caused Por força excessiva de pré-aperto, reduza a força de pré-aperto para um alcance razoável; Se o afrouxamento for causado pela força de pré-aperto insuficiente, aumente a força de pré-aperto e otimize as medidas anti-deenamento ., melhore o projeto da estrutura do parafuso, como aumentar o raio do filete na transição entre a cabeça e o haste para reduzir a concentração de tensão ou o uso de bolts ocos para melhorar a tensão e melhorar a resistência », a falha», com a falha », a falha». process, such as galvanizing, chrome plating or applying anti-corrosion coating, to improve the corrosion resistance of bolts and extend their service life. Adjust the use scenario according to the failure data, replace the easily failed bolts from parts with severe vibration or serious corrosion, and use more suitable bolt types, such as Spiralock thread bolts in parts with large vibration.​

 

  • Como selecionar medidas apropriadas de anti-alojamento do parafuso em diferentes cenários?

Para a seção reta de ferrovias comuns com pequena vibração, pode-se usar um pouco de vibração da arruela de mola, o que tem baixo custo e pode atender às necessidades básicas, e a inspeção regular pode garantir a confiabilidade . de alta velocidade e as ferrovias pesadas e a vibração mais severa, para que a linha de espira ou a espira-espira-lixo e a fútil spirlock seja usada por espira e a espira-lata-{}}}}}}}}}}}} O alojamento anti-se adaptar pode se adaptar à vibração frequente e garantir que os parafusos não se soltem por um longo tempo . peças importantes, como as participação, precisam de um anti-lening de porca dupla . A proteção dupla torna a conexão mais confiável ., mesmo que um cenário Loosens, o outro ainda pode desempenhar um papel de fixing corrosive environments, a composite anti-loosening measure of glue coating and galvanizing should be adopted. While the glue coating prevents loosening, the galvanized layer can resist corrosion and extend the service life of bolts. For parts that are not frequently disassembled, such as track fixing devices, spot welding anti-loosening can be Usado . Depois de instalado, não há necessidade de desmontar, e o efeito anti-alojamento é completo, evitando riscos de afrouxamento .